Céimeanna chun brící sféar alúmana cobhsaí a tháirgeadh go teirmeach

Dec 04, 2024

Ag baint úsáide as réimsí cuas alúmana mar chomhiomláin agus ag cur méideanna cuí SiO2 agus cloch sileacáit leis an maitrís, táirgeadh brící sféar alúmana alúmana le cobhsaíocht turraing teirmeach maith agus ráta athraithe líne lámhaigh íseal.
The main component of ordinary alumina hollow sphere products is Al2O3 (over 98%), and the matrix is composed of α - Al2O3, which is the main raw material causing poor thermal stability of the products. Therefore, when determining the formula, alumina hollow spheres are still used as aggregates, and an appropriate amount of SiO2 is added to the matrix. During the firing process, a certain amount of mullite phase is formed in the matrix to replace corundum phase, thereby improving thermal shock stability. Add a certain amount of silicon wire stone to the matrix to reduce the rate of change in the re firing line of the product and ensure the external dimensions of the product. The use of chemical binders can have adverse effects on the high-temperature performance of products, so chemical binders are not used. From these aspects, the following four formulas have been designed, and the thermal shock stability of their products is in the order of>20 times,>20 uair, 5 huaire, agus 1 uair.

 

 

 

 

 

 

 

Déan teagmháil liom: Ríomhphost: {{1 }/sdwenping@163.com

Teil: 86-0533-4188518 / facs: 86-0533-4188518

Ardaigh: +86-13275332819 (uimhir wechat/whatsapp)

 

Glaoigh Linn
Glaoigh orainn
  • Teil: +86-533-4188518
  • Mob: +8613275332819
  • E - Ríomhphost: sdwenping@163.com
  • Cuir: Seomra 711, Uimh.3, Yanhe Bóthar, Boshan, Zibo, Shandong, Poirceallán